Engineering 185°F - 300°F | Polyphenylene Oxide (PPE)

TECANYL PPE

TECANYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temperature conditions. Chemical attack from water, most salt solutions, acids and bases is also minimal with TECANYL®. The addition of glass fiber reinforcement enhances both the mechanical and thermal properties of the basic TECANYL® material. Made from Noryl® EN265 resin.

  • Good electrical insulating properties
    Due to its extremely low water absorption with values as low as 0.07%, TECANYL® is an excellent electrical insulating material.
  • Long-term dimensional stability
  • Superior impact strength
    TECANYL® has a notched Izod impact strength of 3.5 ft-lbs/in.
  • TECANYL® exhibits a continuous use temperature in excess of 220°F
  • Wide range of UL flammability ratings from
    UL94 HB to UL94 V-1
  • Light weight
    TECANYL®, with a density of 0.0383 lbs/in3, can be used in applications where weight is a significant consideration.
  • Thermoformable capability
  • Possesses good hydrolytic stability

Made from Noryl EN265 resin® exhibits a broad range of outstanding properties for applications in computers and business equipment, automotive, electrical insulation, telecommunications, appliances, electronics, and many other industries.

  Properties Condition Units Value
Physical Chemical Designation PPO
Filler
Density g/cm_ 1.08
Mechanical Tensile Modulus @ 73 °F PSI 350,000
Tensile Strength @ Yld @ 73 °F PSI 9,000
Tensile Strength @ Brk @ 73 °F PSI 9,200
Shear Strength @ 73 °F PSI
Elongation @ Yld @ 73 °F %
Elongation @ Brk @ 73 °F % 25
Flexural Modulus @ 73 °F PSI 370,000
Flexural Strength @ 73 °F PSI 13,400
Compressive Modulus @ 73 °F PSI
Compressive Strength @ 73 °F, 10% strain PSI
Izod (charpy) Impact Strength @ 73 °F ft-lbs/in 3.5
Rockwell Hardness @ 73 °F M (R) Scale (119)
Coefficient of Friction Static 0.39
Coefficient of Friction Dynamic, 40 PSI, 50 FPM 0.32
Wear (K) Factor in_-min/ft-lbs-hr
Limiting PV psi-fpm
Thermal Vicat Softening Point °F 310
Melting Temperature °F
Heat Deflection Temperature @ 66 °F 279
Heat Deflection Temperature @ 264 °F 254
Service Temperature Intermittent °F 230
Service Temperature Long Term °F 220
Thermal Expantion (CLTE) in/in/°F 3.3*10-5
Specific Heat BTU/lb-°F
Thermal Conductivity BTU-in/hr-ft_-°F
Electrical Surface Resistivity ohms/square
Volume Resistivity ohm-cm 1*1017
Dielectric Strength V/mil 500
Dielectric Contant @ 60 HZ, 73 °F, 50% RH 2.7
Dissipation Factor @ 60 Hz, 73 °F 0.0007
Other Moisture Absorption @ 24 hrs, 73 °F % 0.07
Moisture absorption @ Saturation, 73 °F %
Flammability UL 94 V-1
Food Grade N
Relative Cost $